Silver Nanowires Conductive Ink

  • Silver Nanowires Conductive Ink
Silver Nanowires Conductive Ink
  • Description

Product characteristics:
It is made of ultra-fine silver powder and low-temperature curing thermoplastic resin. It is suitable for screen printing of various types of thin film switch conductive lines and has good printing, electrical conductivity, antioxidant properties and excellent adhesion.

Product characteristics:
     

 

     
resultTest Method
     

Solid content

     
     

56%

     
     

Poor quality of baking test for oven

     
     

viscosity(25℃)

     
     

150-200dPa·s

     
     

Rotation viscometer

     
     

Square resistance

     
     

<15mΩ/□

     
     

Resistance meter

     
     

hardness

     
     

≥2H

     
     

Pencil hardness gauge

     
     

adhesion

     
     

Do not fall off

     
     

3M600 tape vertical pull      
     

Bending

     
     

△R≤50%

     
     

It is opposed to the fold and is pressed with a weight of 2 kilograms. It is reserved once a minute. After repeated 10 times, the resistance changes.      

Remarks: The line resistance of the line loop with a length of 1.5 M, a width of 0.6 mm, and a thickness of 3 μm polyester mesh wire is used.

method of application:

1, use: Please use ink knife gently stir, use standard screen printing method silk printing.

2, recommended film thickness: 3 to 5 μm(dry film).

3, screen form: can use 200 to 350 purpose polyester mesh or stainless steel mesh for silk printing.

4, scratch glue: PU scratch glue or other soluble scratch glue, silk printing scratch glue tilt degree 60 to 70 degrees.


Curing method:
After the silver pulp is printed, it must be baked at a low temperature of 130 °C for 30 minutes. The temperature can be higher or longer. The performance of the cured silver line will be better, and it can also be cured by infrared heating furnace.

clean:
Wash with ethyl acetate, butyl acetate and other solvents.

package:
1KG / barrel 5KG / barrel.

Storage conditions and shelf life:
The ideal use period is 6 months after the original tank is delivered(stored at a temperature of 5 to 25 °C).

Previous
Next